It can be seen that at the atomic depth indentation, the hardness
on the single crystal is higher than all the hardness values measured
from nanocrystal samples, which is controversial to classical
H-P size effect observed at bulk material. In previous studies, Ma
et al. [31] suggested that indentation at inner grain or grain boundary
showed a more compliant response and single crystal gave the
stiffest hardness.