The following is a representative procedure for the preparation of the MSF adhesives and XSBRL modified MSF adhesives. MSF adhesives: SF (28 g), tap water (72 g), and crossing-linking agent (12 g) were sequentially added to
a three-neck flask and stirred for 30 min at room temperature. MSF/XSBRL adhesives: Various proportions (0 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%) of XSBRL based on MSF adhesives content were added to the MSF adhesives and further mixed untiluniform at room temperature.