using a smooth bar which allows to deposit 50 lm wet film
onto the substrate. Coating was applied on the sized side of the
paper in order to control the polymer solution penetration. After
coating, the samples were dried overnight at room temperature.
The structure of the packaging material is illustrated in Fig. 1.