the pulp concentration of 9°Brix was optimized as the maximum foam expansion of 72 %, 90 % and 125 % at 0.75 % methyl cellulose, 3 % GMS and 15 % egg white respectively
the pulp concentration of 9°Brix was optimized as the maximum foam expansion of 72 %, 90 % and 125 % at0.75 % methyl cellulose, 3 % GMS and 15 % egg white respectively