For
instance, the encapsulation efficiency and thus, the heat storage
capacity of PS multilayer structures prepared with the lower
amount of electrospun PCL/PCM fibres decreased by up to 100%
for PS multilayer structures stored at 30 days, and between 25%
and 28% for those prepared with the highest amount of PCL/PCM
fibres.
No significant variations were observed in the PS multilayer
structures prepared with both layers (PCL/PCM and PCL fibres) atstructures prepared with both layers (PCL/PCM and PCL fibres) at
4 C. This could be attributed on the one hand, to the physical state