The less corrosion-resistant paint (∼3 g)was mixed with 5 wt% (or in further experiments: 1–10 wt%) ofthe ground polyaniline powders and applied onto a clean sampleof mild steel sample (MS, AISI 1212), 2 cm × 2 cm or 4 cm × 6 cm,using a scalpel-based method