specimens with dimension of 300 mm × 300 mm × 40 mm were sandwiched between the hot plate and the cold plate. Measurements were taken using the device operating on the stationary slab principle at a mean temperature of +20◦C and a temperature gradient of 20◦C. Based on the measurements of the temperature and heat flux difference across the specimen thickness, the thermal conductivity was determined as shown in Eq. (1):