Table 3 shows the results of the analysis of pulp samples selected after each stage of bleaching using Fiber Tester apparatus. The results shown in the table show that the length of the fibers during bleaching insufficiently changed, the values of structure of fibers are significantly high and slightly varied during bleaching. This parameter correlates with mechanical strength [10], as observed in our experiment.