A drop was transferred to a silicon wafer which was
mounted onto an aluminium pin. After the hexane evaporated,
the samples were sputter-coated with 20 nm gold-palladium
(Emitech k550, UK). For imaging the particles in the final aqueous
dispersion, circular 13 mm carbon planchets (Canemco Quebec)
were polished to a mirror finish.