According to Table 4, in terms of quality of peeling, the best
conditions of ohmic peeling were at 25 C and 0.01 g/100 ml NaCl
with 9680 V/m, 60 C and 0.01 g/100 ml NaCl with 9680 V/m and
50 C and 0.01 g/100 ml NaCl with 11,300 V/m. Although quality
was also high at 25 C and 0.01 g/100 ml NaCl with 9680 V/m, the
peeling was slower.