The microstructural investigations for the material conditions of the pipe and also the tube made of nickelbased
Alloy 617 mod. can be summarized as follows (Fig. 6): in the initial state M23C6 precipitates occur within
the grain and at the grain boundaries, in the tube only at the grain boundaries.