Under optimum extrusion conditions, mixed esters are formed, with highest acid value obtained for succinylation of cellulose (0.122 g/g at DS of 0.350) which is two times higher compared to succinylated SD (0.059 g/g at a weight gain of 0.452) and hemicellulose (0.043 g/g at DS of 0.290).