Which interface delaminated, 1st pass or 2nd pass?
Ans:
Dilution of L4503 with LDPE might not give an improvement in bond vs L4210. What is the bond target and what is the bond achieved with Lotader 4210?
Do they still have L4210 in production floor? Can we also try L4210 for test 2 and 3?
Ans:
Has SE Pack tested Lotader 4210 on 2nd pass? What actually trigger them to use L4503 dilution for 2nd pass to replace Nucrel AE? Have them tested Lotader 4210 on 2nd pass?
Ans:
What is the line speed required for test 2 and 3? 150m/min as well?
Ans: