Dear Amy / Barry / Guo Zhong,
I just found that you sent e-mail to my yahoo mail I previously temporary used before new year due to server connection issue.
Thank you so much for comments to action and finding out plating date to continue action.
Based on Amy's email and discussion, please kindly see action as below.
1. Check and confirm to Ya Thai to recalculate the chamber of CASS test - will cooperate with Pla and Santi.
2. We are finding out the plated parts of T1 and T2 of plating date from Barry and Guo Zhong information, check thickness, STEP, pore count, if pass so CASS will be conducted accordingly.
3. Get information of plated parts that passed CASS conducted at Ya Thai (plating on 26 Dec 2013), will check pore count thickness and STEP accordingly.
4. The good parts will be submitted to Enthone China to recheck functional test when new plating lot pass thickness, STEPand pore count.
We are checking thickness of T1 plated on last week and found that thickness of Cu is around lower limit 15 micron (spec > 15 micron), Ni is less than spec > 18 micron and Cr is less than spec > 0.25 micron. STEP and pore count will be conducted soon. So Minth Thailand tested increasing surface area to obtain higher thickness, will update after functional test is finished.
Now we are trying to be familiar with thickness test method at Minth Thailand, Ya Thai, Enthone and Minth thailand will try to complete this action before 24 Jan 2014.