To investigate the ability of biogenic Mn oxides (bio-MnO2) produced in the DHS reactor to adsorb minor metals, Ni(II) and
Co(II) were added in the influent during Phase 7 (day 360e379, almost 3 weeks) at a concentration of 2.5 mg L1 with Mn(II) at 5mg L1.