Subsequently,two different heat treating cycles were used to sinter the samples. A one stage cycle with the sequence heating rate of 5 °C/min up to 900 °C, and
a two stage cycle with the primary sequence heating rate of 5 °C/min up
to 730 °C followed by a secondary sequence heating rate of 1 °C/min up
to 900 °C.