and showed a high dense network microstructure. As shown in
Fig. 7, concrete has very tiny pores and the connectivity of pores
is low. The measured porosity of this concrete only was 8.1% which
Fig. 4. SEM of uncarbonated concrete (G30). much less than samples under lower CO2 concentration condition.