The dimensional stability of kenaf–Kevlar hybrid composites
was determined by water absorption and thickness swelling
test. Three samples of each composite were immersed in distilled
water at room temperature. After a certain period of time,
the samples were removed from the water, wiped with a clean
tissue paper before the weight and thickness value was measured.
The percentage of water absorption was calculated by the
weight difference using the following equation: