In synthesized nano zinc oxide two weight losses were observed, in which first weight loss below
150◦ C was due to water vapourization and second loss around
290 ◦C was due to degradation of nano ZnO. In neem oil blended chitosan/0.5%ZnO/neem oil nanocomposites film three weight loss
were noticeable