These products were taken out of the flask and hotpressed at 1308C and 15 MPa in a window mold andthen were transferred to another cold-press machineand molded at room temperature. According to the increases in the molecular weight, the prepolymers werenamed p1,p2, and p3, and the corresponding elastomers were named e1,e2, and e3