The fiber is produced using sugarcane bagasse as 5 percent of replacement sand and do not need to add aluminum powder. In such conditions found. Aerated concrete has a compressive strength of 7.22 MPa the density of 1368.4 ± 74.23kg / M3. And the water absorption of 10.32%.