tear tests were cut from the rubber vulcanized sheets having thickness
of about 1 mm using die C and die B, respectively.
The specimens were tested using a 1 kN load cell and a crosshead
speed of 500 mm/min. In addition, the tensile
strength of the vulcanizates before and after aging was
compared to give a measure of aging resistance