The strengthened and repaired columns failed in a ductile
manner characterized by the larger area enclosed by the
load displacement curve at the end of the test compared
to a brittle failure in case of control columns. However,
the repaired failed columns showed a significant loss in
ductility due to the existence of cracks in failed columns.