The purpose of this paper is to analyze the influence of processing parameters: slab thickness, water flow of interstand cooling and oil flow in roll gap lubrication system, on the formation of the tertiary scale during hot strip rolling of low-carbon steel in factory. The scale occurrence is discussed considering two aspects: thickness and composition.