For the oxidation studies of the ceramic monoliths, samples with
a diameter of 7.5 mm and thickness of 2.2 mm were ground and
polished with diamond paste to sub- m roughness; subsequently,
the polished samples were cleaned in acetone using ultrasound
and dried at 100 ◦ C in the oven. The oxidation test of the ceramic