. After being treated by ethanol at
three different temperatures, the maximal FAME yields for the M-CaO
catalysts were 94.4%, 96.2% and 92.9%, respectively (U-CaO, 87.5%).
The superior performance of catalyst was due to the high specific basicity,
high surface area and porosity, and small crystalline size