This might be due to the
well co-condensed LMWPF and UF resin at the glue line during the
gluing process. However, a previous study by Lee and Kim [32]
showed, from NMR analysis, that there was no significant co-condensation
between urea and phenolic units with the different
urea addition methods during the synthesis of PUF resin.