Results
indicated that in terms of quality of peeling, the best conditions of ohmic peeling were: 0.01 g/100 ml
NaCl with 8060 and 9680 V/m, and 0.03 g/100 ml NaCl with 6450 and 8060 V/m. These conditions
showed potential for processing because they required a reasonably short time (approximately 1 min)