Then, the coagulated rubber was sheeted with a creping
machine, washed with water and dried in an oven at 50 C
to produce silica/NR masterbatch. In addition, coagulated
NR without silica was also prepared in the same manner as
the silica/NR masterbatches and used as the raw rubber for
the conventional mixes.
Since it was possible that