The pellets of both PLA and PCL were initially dried in vacuum oven at a temperature of 50oC for 2 days to remove the absorbed moisture, before processing through Rheomex.
The pellets of both PLA and PCL were initially dried in vacuum oven at a temperature of 50oC for 2 days toremove the absorbed moisture, before processing through Rheomex.