Visual inspection of welds in all steels may begin immediately after the completed welds have cooled to ambient
temperature .Acceptance criteria for ASTM A514,A517, and A709 Grade HPS 100W [HPS 690W] steels shall
be based on visual inspection performed not less than 48 hours after completion of the weld.