Purified fraction of the iron-chromium catalyst with a grain size of 75–150 μm is a material, which undergoes stable fluidization. Experimentally determined minimum fluidization velocity allowed to select the necessary molar flow rate of substrates. Thanks to proper dilution system of the products stream, the laboratory installation enabled online reaction monitoring with an FTIR spectrometer.