The prepared SLN dispersions were kept in the dark condition at three different temperatures of 4, 25, and 40 8C. After 60 days of storage, a gelation was visually observed for all samples, especially for those stored at 40 8C. Since the prepared SLNs had large particle diameter and high values of PDI, the instability induced by the gelation could take place over storage. The observed instability of