3.3. Static Loads Test Results
The cylindrical steel static loads are added one by one on the surface of the SMC roof tile as shown in Figure 3 (b) until the failure condition, i.e. cracks. Cracks occurred in locations where there a stress concentration occurs, at the sharp bends in the lines at peaks or valleys of roof tile as shown in Fig. 6.