Even though both
catalysts demonstrated almost similar degradation efficiency, the
reaction rate was exactly different at the beginning of the reaction
as Fe (II)/Y possessed quite higher degradation rate compared to Fe
(III)/Y catalysts between the first 30 and 60 min.