The anode and cathode
materials used to make the full cells were TIMREX SLP 30 graphite
and LiNi1/3Co1/3Mn1/3O2 (NCM) (Toda NCM-01ST-100), respectively.
The electrolyte used was 1 M LiPF6 in ethylene carbonate (EC)/
dimethyl carbonate (DMC) 1:1 (v/v) (Novolyte Technologies).