Our hypothesis shares similarities with that proposed by Fairclough and Conti (2009) who suggest that rapid decompression of PP film (from a maximum temperature of 86 °C) results in explosive decompression
of solubilized gas within the material, leading to opaque areas on the film due to light-scattering microscopic pits and bubbles.