The TGA–DTA curves of the as-spun nanofibers are presented in Fig. 3. The figure shows three major weight loss events in the fibers. The first weight loss of 7 wt% occurred between 30 and 200 1C because of evaporation of residual moisture and ethanol molecules in the fibers.