The mechanical properties of the composites were measured
before and after 120 h of thermal oxidation exposure at 80 C [13].
At least five dumbbell-shaped tensile samples were tested for each
kind of composite. The mechanical tests were carried out according
to Chinese standard GB/T 528e2009.