The particle of MP-LRS3 was smaller and relatively smoother while UP-LRS3 was bigger and
rougher compared to GP-LRS3. Among these samples, GP-LRS3 exhibited the highest degree of ordered
structure and crystallinity, the amorphous region of MP-LRS3 was the biggest and UP-LRS3 displayed
the highest degree of double helical structure