This is due to at a longer CO2 activation time, there is an sufficient amount of CO2 reacting with the carbon to produce pores, while at higher KOH/Chare ratio, the more severe etch of the wall takes place to create a great quantity of micropores, resulting in an increase in the pore volume and the high BTE is obtained.