Demould specimens to be tested at 24 h just before testing.
Demould specimens to be tested at greater ages within the period 16 h to 28 h after the addition of water to the other constituents in the mix unless the concrete has not achieved sufficient strength to enable specimens to be demoulded during this period. In such cases, delay demoulding for a further 24 h.