2.2. Peel-off Tests
2.2.1. Variation of the Ag content
To obtain sufficient long-term reliability of the modules during the thermo-mechanical stress during operation, a
good adhesion of the soldering ribbons to the cells is essential. In peel-off tests, a minimum peel-off force of 1 N
per mm ribbon width needs to be obtained.
Fig.