DTG graphs for EFB display two distinctive peaks, in which the first peak is 0.22-0.62 mg/s
lower than the next. The first peak corresponds to the degradation of lower molecular weights
components (hemicellulose) from 180o
C to 310°C and second peaks indicates cellulose degradation
which occurs between 320o
C and 410°C