Appropriate RDF production process consists of manual sorting, magnetic separation, bag
breaking/homogenization, screening with the opening of 40 mm, air drying, shredding and
palletizing. This process can produce RDF that has average lower heating value (LHV)
around 19.6 MJ/kg at 12% moisture content. Chlorine and sulfur contents are 0.6% and
0.2% respectively. Heavy metals such as Cd, Cr, Hg and Pb do not exceed European RDF
standard. The RDF consists of more than 40% plastic, 30% yard waste, less than 10%
paper, 10% food waste and 10% noncombustible fraction. Cost of RDF production to get
required characteristics mentioned earlier is also provided for decision makers and
investor