Electrospun fibers with the addition of LENRA have the smallest
diameter and the highest degradation temperature within the natural rubber’s group due to the presence of acrylate
and epoxy group. The bead formation is increases when LNR was added into the fibers due to lack of interaction
between the PVC and LNR.