The brown
incompletely carbonized biomass generated was then ground in
a laboratory mortar to form fine powder, which was mixed with
200 mL of concentrated sulphuric acid (95–97%) in a round bottomed
flask fitted with a condenser and subsequently heated at
150 C for 15 h under nitrogen.