A DSSC is formed of a nanocrystalline metal oxide semiconducting layer deposited on transparent fluorine doped tin oxide (FTO) conductive glass, adsorbed dye on the semiconducting material, counter electrode, and an electrolyte containing iodide and triiodide ions