For full specimen, the location of the fatigue crack initiation site was determined by comparing the observation on both fracture surface by SEM and outside surface by OM, and the results for each specimen are listed in Table 3. From 16 failed full specimens in this test, 14 failed at the TMAZ on the advancing side and 2 at the NZ.