In order to synthesize silver nanoparticles (SNPs), 10 mL of the leaf extract was mixed with 90 mL of 1 mM silver nitrate solution and heated in a water bath, set at 80 °C for 10 min. A color change from yellow to brown designates the formation of colloidal SNPs.